Preparation and Aqueous Durability of Sr Incorporation into Rutile TiO2

Preparation and Aqueous Durability of Sr Incorporation into Rutile TiO2

https://devfeature-collection.sl.nsw.gov.au/record/TN_cdi_proquest_journals_1750392358

Preparation and Aqueous Durability of Sr Incorporation into Rutile TiO2

About this item

Full title

Preparation and Aqueous Durability of Sr Incorporation into Rutile TiO2

Publisher

Wuhan: Wuhan University of Technology

Journal title

Journal of Wuhan University of Technology. Materials science edition, 2015-12, Vol.30 (6), p.1179-1183

Language

English

Formats

Publication information

Publisher

Wuhan: Wuhan University of Technology

More information

Scope and Contents

Contents

TiO2 was employed as the waste form for disposal of simulated nuclide Sr. Preparation of Sr bearing rutile was explored under different sintering temperatures and Sr contents. The optimal treatment temperature was confirmed as 1300 ℃ for the incorporation of SrO in rutile Ti O2. Perovskite type Sr TiO3 was prepared as the resultant product. The lim...

Alternative Titles

Full title

Preparation and Aqueous Durability of Sr Incorporation into Rutile TiO2

Authors, Artists and Contributors

Identifiers

Primary Identifiers

Record Identifier

TN_cdi_proquest_journals_1750392358

Permalink

https://devfeature-collection.sl.nsw.gov.au/record/TN_cdi_proquest_journals_1750392358

Other Identifiers

ISSN

1000-2413

E-ISSN

1993-0437

DOI

10.1007/s11595-015-1292-5

How to access this item