Log in to save to my catalogue

Nominally Anaerobic Corrosion of Carbon Steel in Near-Neutral pH Saline Environments

Nominally Anaerobic Corrosion of Carbon Steel in Near-Neutral pH Saline Environments

https://devfeature-collection.sl.nsw.gov.au/record/TN_cdi_proquest_journals_2421533679

Nominally Anaerobic Corrosion of Carbon Steel in Near-Neutral pH Saline Environments

About this item

Full title

Nominally Anaerobic Corrosion of Carbon Steel in Near-Neutral pH Saline Environments

Publisher

Houston, TX: NACE International

Journal title

Corrosion (Houston, Tex.), 2010-04, Vol.66 (4), p.45001-45001-11

Language

English

Formats

Publication information

Publisher

Houston, TX: NACE International

More information

Scope and Contents

Contents

Gas transmission pipeline corrosion commences when coatings disbond, exposing the steel to groundwater. When this occurs, a number of anaerobic and aerobic corrosion scenarios can be envisaged. The initial nominally anaerobic corrosion period has been investigated by applying a combination of electrochemical methods (i.e., corrosion potential, line...

Alternative Titles

Full title

Nominally Anaerobic Corrosion of Carbon Steel in Near-Neutral pH Saline Environments

Authors, Artists and Contributors

Identifiers

Primary Identifiers

Record Identifier

TN_cdi_proquest_journals_2421533679

Permalink

https://devfeature-collection.sl.nsw.gov.au/record/TN_cdi_proquest_journals_2421533679

Other Identifiers

ISSN

0010-9312

E-ISSN

1938-159X

DOI

10.5006/1.3381566

How to access this item